Skip to content
  • الرئيسية
  • +972599244055
  • ENGLISH

* ELit

Brand:

GEKA

Model:

ELIT

Standards
TS EN ISO 2560-AE 42 0 RR 1 2
EN ISO 2560-AE 42 0 RR 1 2
AWS A5.1E6013
Chemical Composition of Weld Metal % (Typical)
CSiMn
0.070.30.5
Typical Base Material Grades
  • S235JR, S275JR, S235J2G3-S355J2G3, S235JRS1 – S235J2S1, S235JRS2 – S235J2S2, S235JRS1 – S235J2S1, S235JRS2 – S235J2S2
  • P235GH, P265GH, P255NH, P235T1 – P355T1, P235T2 – P355T2, P235G1TH, P255G1TH
  • L210 – L360NB
Mechanical Properties
Yield Strength (N/mm²)Tensile Strength (N/mm²)Impact Strength (ISO-V/ 0°C)Elongation ((Lo=5do) (%))
min. 420510-610min. 47 Jmin.22
Features and Applications
  • The mostly used type among the rutile electrodes
  • Easy striking
  • Spatter and fume formation in low amounts
  • Good welding beads
  • Electrode coating of high thickness
Current Type
  • AC
  • DC(-)
Operating Data
Product CodeDiametré x Length (mm)Diameter x Length (inch)Welding Current (A)Weight g / 100 pcs
3010100003ø2,0 x 300ø5/64 x 1245 – 801160
3010100012ø2,5 x 350ø3/32 x 1460 – 1102000
3010100018ø3,2 x 350ø1/8 x 14100 – 1403220
3010100024ø4,0 x 350ø5/32 x 14140 – 1804740
3010100027ø4,0 x 450ø5/32 x 18140 – 1806220
3010100030ø5,0 x 350ø3/16 x 14170 – 2407640
3010100033ø5,0 x 450ø3/16 x 18170 – 2409680
Approvals
ABS-BV-CE-DB-DNV-GL-LR-RI-NA –TL–TSE-UKR -SEPRO-VdTUV-NK

نسخة PDF

* ELOX R 309 L

TS EN ISO 3581-AE 23 12 L R 3 2
TS EN ISO 3581-AE 23 12 L R 3 2
AWS A5.4E309L-16
Chemical Composition of Weld Metal % (Typical)
CSiMnCrNi
0,030,80,823,012,6
Typical Base Material Grades
  • Used for buffer layer unalloyed or low alloyed steels, also when joining non-molibdenum-alloyed stainless and carbon steels. Joints and mixed joints between austenitic steels.
  • Used for mixed joints between austenitic and heat resistant steels.
Mechanical Properties
Yield Strength (N/mm²)Tensile Strength (N/mm²)Impact Strength (ISO-V/+20°C)Elongation ((Lo=5do) (%))
min. 440540 – 720min.47 Jmin. 30
Features and Applications
  • GeKa ELOX R 309L electrodes are widely used in carbon-stainless steel joints. for example, joining mild or low alloy steels with AISI 304.
  • If a service temperature above 370 °C or heat treatment is applied after welding dissimilar steels, embrittlement or cracking may occur. This requires procedural control.
  • Ferrite content of weld metal is greater than 8 FN and reduces the possibility of intergranular carbide precipitation. This thereby increases the resistance to intergranular corrosion without the use of niobium.
  • Re-drying: 120-200ºC / 2 h.
Current Type
  • AC
  • DC(+)
Operating Data
Product CodeDiametré x Length (mm)Diameter x Length (inch)Welding Current (A)Weight g / 100 pcs
3010101058ø2,0 x 250ø5/64 x 1050 – 85950
3010101063ø2,5 x 250ø3/32 x 1060 – 901540
3010101073ø3,2 x 350ø1/8 x 1480 – 1203610
3010101078ø4,0 x 350ø5/32 x 14100 – 1605290
Approvals
ABS-BV-CE-TSE-UKR-SEPRO

نسخة PDF

* ELOX R 316 L

TS EN ISO 3581-AE 19 12 3 L R 3 2
EN ISO 3581-AE 19 12 3 L R 3 2
AWS A5.4E316L-16
Chemical Composition of Weld Metal % (Typical)
CSiMnCrNiMo
0,030,80,919,011,52,6
Typical Base Material Grades
  • EN: X2CrNiMo17-12-2, X2CrNiMo18-14-3, X3CrNiMo17-13-3, X5CrNiMo17-12-2, X6CrNiMoTi17-12-2, X6CrNiMoNb17-12-2, X10CrNiMoNb18-12, G-X2CrNiMo19-11-2
  • AISI: 316L, 316Ti, 316Cb
Features and Applications
  • Tanks, pipes and equipments made of Cr-Ni-Mo low-carbon steels which are used in food, textile, chemical and paint industries
  • Weld metal is resistant to acid, corrosion
  • Serviceability at temperatures up to 400°C
  • Requirement of Re-drying for min. 2 hours at the temperature 300°C
Mechanical Properties
Yield Strength (N/mm²)Tensile Strength (N/mm²)Impact Strength (ISO-V/+20°C)Elongation ((Lo=5do) (%))
min. 355540-670min. 47 Jmin. 30
Current Type
  • AC
  • DC(+)
Operating Data
Product CodeDiametré x Length (mm)Diameter x Length (inch)Welding Current (A)Weight g / 100 pcs
3010101243Ø2,0 x 250Ø5/64 x 1040 – 70950
3010101248Ø2,5 x 250Ø3/32 x 1050 – 901500
3010101258Ø3,2 x 350Ø1/8 x 1480 – 1203480
3010101263Ø4,0 x 350Ø5/32 x 14110 – 1605130
Approvals
ABS-BV-CE-TSE-UKR-SEPRO

نسخة PDF

بإمكانك مراسلتنا لإستشارات البناء

  • فلسطين - غزة
  • * شارع صلاح الدين
  • * جوال : +972599410805
  • * جوال :+972599244055
  • * مكتب : +97082051371
bassam AlMassri Co. for General Trading
By SKT Free Themes
  • ←
  • WhatsApp
  • Phone